The corrosion resistance of conventional and high alloy stainless steels (specifically 316L, 317L, 904L, duplex 2205, 3127hMO, 1925hMO, 254SMO, 654SMO and Remanit-4565) was determined electrochemically in chlorinated and unchlorinated Arabian Gulf Seawater at 25 and 50 °C. The stainless steels 316L and 317L were used as reference alloys. The electrochemical potentiodynamic cyclic polarization method was used to determine the passive film break down potential ( E b), protection potential ( E prot) and maximum current attained on scan reversal ( I max). It was found that at 25 °C in chlorinated and unchlorinated seawater and at 50 °C in unchlorinated seawater, stainless steels 316L and 317L have poor resistance to corrosion, Stainless steels 904L and duplex 2205 at 25 °C in chlorinated and unchlorinated seawater showed good resistance to corrosion but at 50 °C these steels failed to resist. The high alloy stainless steels such as 3127hMO, 1925hMO, 254SMO, 654SMO and Remanit-4565 showed better corrosion resistance under all the test conditions.
|